Steel 35KHGL

Designation

Name The value
Designation GOST Cyrillic 35ХГЛ
Designation GOST Latin 35XGL
Transliteration 35HGL
The chemical elements 35CrMn

Description

35KHGL steel is used: for the manufacture of castings to various industrial purpose.

Standards

Name Code Standards
Castings, steel В82 GOST 977-88

Chemical composition

Standard C S P Mn Cr Si Fe
GOST 977-88 0.3-0.45 ≤0.04 ≤0.04 0.6-0.9 0.5-0.8 0.5-0.75 The rest
Fe is the basis.

Mechanical characteristics

Section, mm sT|s0,2, MPa σB, MPa d y, % kJ/m2, кДж/м2
Hardening in air, 840-860 °C + vacation at 500-680 °C, air cooling
100 ≥383 ≥726 ≥10 ≥20 ≥167
Normalization at 850-880 °C + Vacation at 550-650 °C, air cooling
100 ≥334 ≥628 ≥14 ≥25 ≥137

Description mechanical marks

Name Description
Section Section
sT|s0,2 Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2%
σB Limit short-term strength
d Elongation after rupture
y The relative narrowing
kJ/m2 Toughness