Steel 30KH3S3GML

Designation

Name The value
Designation GOST Cyrillic 30Х3С3ГМЛ
Designation GOST Latin 30X3C3GML
Transliteration 30H3S3GML
The chemical elements 30Cr3С3MnMo

Description

30KH3S3GML steel is used: for the manufacture of castings of highly loaded parts for critical applications with wall thickness up to 30 mm, which meet the requirement of high strength and sufficient toughness.

Standards

Name Code Standards
Castings, steel В82 GOST 977-88

Chemical composition

Standard C S P Mn Cr Si Fe Mo
GOST 977-88 0.29-0.33 ≤0.02 ≤0.02 0.7-1.2 2.8-3.2 2.8-3.2 The rest 0.5-0.6
Fe is the basis.

Mechanical characteristics

Section, mm sT|s0,2, MPa σB, MPa d5, % y, % kJ/m2, кДж/м2
Normalization at 970-990 °C + vacation at 700-720 °C, air cooling + tempering air from 980-1000 °C + vacation at 200-220 °C, air cooling
100 ≥1472 ≥1766 ≥4 ≥15 ≥196

Description mechanical marks

Name Description
Section Section
sT|s0,2 Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2%
σB Limit short-term strength
d5 Elongation after rupture
y The relative narrowing
kJ/m2 Toughness