HN35WTJU sheet, strip, foil, plate
Equivalent
Grade | analogue | W. Nr. | Aisi Uns | En | Order |
---|---|---|---|---|---|
KhN35VTYU | EI787 | Buy from stock, view availability |
Supplier
«Auremo» supplier offers to buy products on the most faborable terms by wholesale. There is a wide range of half-finished goods in stock. Strip, sheet, foil of HN35WTJU are always in stock. You can buy goods for an affordable price from HN35WTJU sheet, strip supplier. A wide range of goods for scaled-up fabrications is always in stock. Buy HN35WTJU sheet, strip right now!
Technical characteristics
Steel of grade HN35WTJU is a high-alloyed heat-resistant alloy on an iron-nickel basis. It is used in manufacture of floating details that work at temperatures of 900−1000°C. This alloy relates to a category of ferritic-austenic steels. In comparison with austenic steels, it has almost twice as large strength, higher resistance to intercrystalline corrosion, increased resistance to corrosion cracking in alkaline and chloride environment. A usage of austenic and ferritic steels directly depends on conditions of exploitation.
Manufacture
An iron basis is alloyed with 34−38% of nickel, 14−16% of chrome. Titanium (1,1−1,5%), copper (<0.25%), phosphorus (<0.03%), mangan (<1-2%), wolframium (2,3-3,5%), molybdenum (<0,3%), sulfur (0,02%) should be added to charge mixture in the capacity of masteralloys.
Chemical composition
GOST | Cr | Ni | W | Mn | Ti | Si | Cu | Mo | P | Fe | S |
5632−72 | 14−16 | 34−38 | 2.3−3.5 | 1.0−2.0 | 1.1−1.5 | <0,6 | <0,25 | <0,3 | <0,03 | the rest | <0,02 |
Alloy smelts in open electric furnaces with a help of vacuum arc remelting. Jumping-up temperature of semi-fabricates is 1170 °C at the beginning; in the end a temperature is 850 °C. A finished product cools in the air.
Dimension | Direction | sв |
sT |
d5 |
y | KCU |
MPa | MPa | % | % | kJ/m2 | ||
Bar | Longitudinal | 1050 | 700 | 7 | 10 | 250 |
Welding
Type | Description |
limitedly weldable | welding is possible at heating to 100−120°С and last heat treating |
hardly weldable | in order to obtain a qualitative welded joints, it is necessary to perform the following operations: while welding to heat it up to 200−300°C, to do a heat treatment (annealing) after welding |
weldable without stint |
welding is done without further heat treating or previous heating |
Application
This alloy is used in manufacture of disks, compressor rotor blades, gas-turbine engine with a limited service life at a temperature of 550−750°С.
Buy at a bargain price
«Auremo» is HN35WTJU sheet, strip supplier of precision mill-products to countries of Eastern and Central Europe. An experience of our company allows you easily buy HN35WTJU sheet, strip. A wide selection of products is presented in catalog. Strip, sheet, foil HN35WTJU are always in stock. HN35WTJU sheet, strip price depends on order quantity and additional conditions of supply. HN35WTJU sheet, strip price is privileged for wholesale customers. We are working with the experienced managers. We have the best price-quality ratio. We invite you to a partnership.