By visiting this site, you accept the use of cookies. More about our cookie policy.

Steel 12DKHN1MFL

Designation

Name The value
Designation GOST Cyrillic 12ДХН1МФЛ
Designation GOST Latin 12DXH1MFL
Transliteration 12DHN1MFL
The chemical elements 12CuCrН1MoV

Description

12DKHN1MFL steel is used: for the manufacture of litho-welded structures, castings for critical loaded parts, which are requirements of sufficient strength and toughness, working under static and dynamic loads.

Standards

Name Code Standards
Castings, steel В82 GOST 977-88, OST 3-4365-79

Chemical composition

Standard C S P Mn Cr Si Ni Fe Cu V Mo
GOST 977-88 0.1-0.18 ≤0.03 ≤0.03 0.3-0.55 1.2-1.7 0.2-0.4 1.4-1.8 The rest 0.4-0.65 0.08-0.15 0.2-0.3
Fe is the basis.

Mechanical characteristics

Section, mm sT|s0,2, MPa σB, MPa d5, % y, % kJ/m2, кДж/м2 Brinell hardness number, MPa
Hardening in air, 890-910 °C + vacation at 520-630 °C, air cooling
100 ≥735 ≥981 ≥10 ≥20 ≥294 -
Normalization at 940-960 °C, air cooling or Normalizing at 890-910 °C + vacation at 520-630 °C, air cooling
100 ≥638 ≥785 ≥12 ≥20 ≥294 217-269

Description mechanical marks

Name Description
Section Section
sT|s0,2 Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2%
σB Limit short-term strength
d5 Elongation after rupture
y The relative narrowing
kJ/m2 Toughness