By visiting this site, you accept the use of cookies. More about our cookie policy.

Steel 30KHL

Designation

Name The value
Designation GOST Cyrillic 30ХЛ
Designation GOST Latin 30XL
Transliteration 30HL
The chemical elements 30Cr

Description

30KHL steel is used: for the manufacture of castings of the housings are shock-absorbing devices of freight cars, and other parts of various industrial; hinged cast normal strength chains for rotary kilns used in cold area when the gas stream temperature of 200−500° C and a heat exchange device of rotary cement kilns.

Standards

Name Code Standards
Castings with special properties (cast iron and steel) В83 GOST 21357-87, TU 4112-07507311-010-02
Castings, steel В82 GOST 977-88

Chemical composition

Standard C S P Mn Cr Si Ni Fe Cu
GOST 977-88 0.25-0.35 ≤0.04 ≤0.04 0.5-0.9 0.5-0.8 0.2-0.5 - The rest -
GOST 21357-87 0.25-0.35 ≤0.02 ≤0.02 0.5-0.9 0.5-0.8 0.2-0.5 ≤0.3 The rest ≤0.3
Fe is the basis.

Mechanical characteristics

Section, mm sT|s0,2, MPa σB, MPa d y, % kJ/m2, кДж/м2
Hardening in air, 890-910 °C + vacation at 620-660 °C, air cooling
100 ≥432 ≥677 ≥15 ≥30 ≥402
Normalization at 900-920 °C + vacation at 550-650 °C, air cooling
100 ≥285 ≥530 ≥15 ≥30 ≥265
Casting. Quenching in water from 920-950 °C + vacation at 600-650 °C, air cooling (KCU-60)
- ≥550 ≥660 ≥10 ≥20 ≥3

Description mechanical marks

Name Description
Section Section
sT|s0,2 Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2%
σB Limit short-term strength
d Elongation after rupture
y The relative narrowing
kJ/m2 Toughness