Steel 23KHGS2MFL

Designation

Name The value
Designation GOST Cyrillic 23ХГС2МФЛ
Designation GOST Latin 23XGC2MFL
Transliteration 23HGS2MFL
The chemical elements 23CrMnС2MoV

Description

23KHGS2MFL steel is used: for the manufacture of casting parts for critical applications with wall thickness up to 30 mm, operating under cyclic and shock loads in conditions of impact-abrasive wear.

Standards

Name Code Standards
Castings, steel В82 GOST 977-88, OST 3-4365-79

Chemical composition

Standard C S P Mn Cr Si Fe V Mo
GOST 977-88 0.18-0.24 ≤0.025 ≤0.025 0.5-0.8 0.6-0.9 1.8-2 The rest 0.1-0.15 0.25-0.3
Fe is the basis.

Mechanical characteristics

Section, mm sT|s0,2, MPa σB, MPa d5, % y, % kJ/m2, кДж/м2
Normalization at 1000-1040 °C + vacation at 720-740 °C, air cooling + tempering air from 1000-1020 °C + vacation at 180-220 °C, air cooling
100 ≥1079 ≥1275 ≥6 ≥24 ≥392

Description mechanical marks

Name Description
Section Section
sT|s0,2 Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2%
σB Limit short-term strength
d5 Elongation after rupture
y The relative narrowing
kJ/m2 Toughness