Steel 25ГСЛ

Designation

Name The value
Designation GOST Cyrillic 25ГСЛ
Designation GOST Latin 25GCL
Transliteration 25GSL
The chemical elements 25MnС

Description

25ГСЛ steel is used: for the manufacture of castings of blades of hydraulic turbines, gear rims and wheels, bushings, sectors, columns, details of welded-cast structures with a large amount of welding.

Chemical composition

Standard C S P Mn Cr Si Ni Cu
0.22-0.28 ≤0.3 ≤0.3 1-1.3 ≤0.3 0.6-0.8 ≤0.3 ≤0.3
Chemical composition is not verified by NTD. Total verified brands for chemical compounds: 2906 of 3316.

Mechanical characteristics

Section, mm sT|s0,2, MPa σB, MPa d5, % d kJ/m2, кДж/м2 Brinell hardness number, MPa
Annealing in air 85-900 °C + vacation at 650 °C, air cooling
20 ≥560 ≥710 - ≥43 ≥860 207
Normalization at 900-920 °C + vacation at 580-600 °C, air cooling
100 ≥245 ≥470 ≥18 ≥30 ≥290 123-149
Normalization at 900-920 °C, air cooling
20 ≥350 ≥540 - ≥32 ≥650 170

Description mechanical marks

Name Description
Section Section
sT|s0,2 Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2%
σB Limit short-term strength
d5 Elongation after rupture
d Elongation after rupture
kJ/m2 Toughness

Technological properties

Name The value
Weldability welded without any restrictions. Welding methods: SMAW, ADS under gas protection electroslag welding
Propensity to temper brittleness tend not
Flock-sensitive sensitivity not sensitive
Workability by cutting In a normalized state in HB 156 and blower SB=510 MPa Kn TV.SPL.=1.0 Kn b.St.=0.9

Our consultant will save your time