Description

Alloy ВТ4 used: for the production of parts for various purposes, operating at temperatures up to 400 °C.

Note

Alloy with high corrosion resistance.

Standards

Name Code Standards
Non-ferrous metals, including rare metals, and their alloys В51 OST 1 90000-70
Bars В55 OST 1 90107-73
Sheets and stripes В53 TU 14-1-3444-82

Mechanical characteristics

Section, mm σB, MPa d5, % y, % kJ/m2, кДж/м2 Brinell hardness number, MPa
Forgings weighing up to 200 kg after annealing
101-250 785-1030 ≥8 ≥18 ≥294 241-321
100 834-1030 ≥10 ≥30 ≥343 241-321
Forged square bars and round after annealing
140-250 785-1030 ≥8.5 ≥20 ≥294 241-321
804-1030 ≥9 ≥25 ≥294 241-321

Description mechanical marks

Name Description
Section Section
σB Limit short-term strength
d5 Elongation after rupture
y The relative narrowing
kJ/m2 Toughness

Our consultant will save your time

+49(1523) 72 15 100
E-mail:
Telegram:
WhatsApp:

Subscription

Special offers and discounts. :)