Steel 20KH25N19S2L (15Х25Н19С2Л)
Designation
| Name |
The value |
| Designation GOST Cyrillic |
20Х25Н19С2Л |
| Designation GOST Latin |
20X25H19C2L |
| Transliteration |
20H25N19S2L |
| The chemical elements |
20Cr25Н19С2 |
| Name |
The value |
| Designation GOST Cyrillic |
15Х25Н19С2Л |
| Designation GOST Latin |
15X25H19C2L |
| Transliteration |
15H25N19S2L |
| The chemical elements |
15Cr25Н19С2 |
Description
20KH25N19S2L steel is used: for the manufacture of castings of parts operating at high temperatures in a highly stressed condition (retorts for annealing, heat treatment furnaces and parts boxes for carburizing); tsentrobezhnolityh pipes used as components in equipment for metallurgical, engineering, glass, ceramic, mining and processing petrochemical industry and is intended for the manufacture of blanks and parts used in the composition of the products of aviation and the nuclear industry.
Note
Steel corrosion resistant austenitic, heat resistant up to +1100 °C.
Standards
| Name |
Code |
Standards |
| Castings with special properties (cast iron and steel) |
В83 |
GOST 2176-77, TU 14-1-959-74 |
| Castings, steel |
В82 |
GOST 977-88, OST 24.920.01-80, OST 3-4365-79 |
| Pipes steel and connecting parts to them |
В62 |
TU 1333-003-76886532-2014 |
Chemical composition
| Standard |
C |
S |
P |
Mn |
Cr |
Si |
Ni |
Fe |
Cu |
| TU 1333-003-76886532-2014 |
≤0.2 |
≤0.03 |
≤0.035 |
0.5-1.5 |
23-27 |
2-3 |
18-20 |
The rest |
- |
| GOST 2176-77 |
≤0.2 |
≤0.03 |
≤0.035 |
0.5-1.5 |
23-27 |
2-3 |
18-20 |
The rest |
≤0.3 |
Fe is the basis.
According to GOST 2176-77, the chemical composition is given for steel grade 20Х25Н19С2Л. Deviations from the norms of chemical composition are allowed: for carbon ± 0.020%; for silicon ± 0.10%; on manganese, copper, chromium and nickel ± 0.10% each; by titanium and tungsten ± 0.050% each; by vanadium, molybdenum and niobium ± 0.020% each.
Mechanical characteristics
| Section, mm |
sT|s0,2, MPa |
σB, MPa |
d5, % |
y, % |
| Casting. Quenching in water, oil or air with 1090-1110 °C |
| 100 |
≥245 |
≥491 |
≥25 |
≥28 |
| Casting. Normalization at 1100-1150 °C, air cooling |
| - |
≥245 |
≥490 |
≥20 |
≥25 |
Description mechanical marks
| Name |
Description |
| Section |
Section |
| sT|s0,2 |
Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2% |
| σB |
Limit short-term strength |
| d5 |
Elongation after rupture |
| y |
The relative narrowing |