Designation
Name | The value |
---|---|
Designation GOST Cyrillic | РС-5406 |
Designation GOST Latin | PC-5406 |
Transliteration | RS-5406 |
The chemical elements | - |
Description
Alloy RS-5406 is used: for the manufacture by vacuum-thermal deposition of thermally stable, thin-film resistive elements and various auxiliary layers of electronic devices; for low-impedance resistive layers with a wide range of resistivity and positive temperature coefficient of resistance of the order of 10-5 deg-1, with corrosion resistance and ability to adhesion, a method of explosive evaporation from the tungsten evaporator.
Note
Silicon alloy resistive.
Standards
Name | Code | Standards |
---|---|---|
Solid alloys, metal-ceramic products and powders, metal | В56 | GOST 22025-76 |
Chemical composition
Standard | C | Cr | Si | N | O | Co | H |
---|---|---|---|---|---|---|---|
GOST 22025-76 | ≤0.06 | 52.5-55.5 | The rest | ≤0.02 | ≤0.3 | 4.5-7.5 | ≤0.003 |
Cr is the basis.