By visiting this site, you accept the use of cookies. More about our cookie policy.

Steel 7Х2СМФ

Designation

Name The value
Designation GOST Cyrillic 7Х2СМФ
Designation GOST Latin 7X2CMF
Transliteration 7H2SMF
The chemical elements 7Cr2СMoV

Description

7Х2СМФ steel is used: for the manufacture of forged work rolls for cold rolling of metals.

Chemical composition

Standard C S P Mn Cr Si Ni Fe V Mo
0.7-0.8 ≤0.03 ≤0.03 0.6-1 1.7-2.2 0.7-1 ≤0.5 The rest 0.15-0.3 0.35-0.6
Fe is the basis.

Technological properties

Name The value
Forging temperature Start - 1200 °C, the end - of 800 °C.