Steel AS40
Steel AC35G2
AC20X steel
Steel АЦ20ХГНМ
Steel АЦ20ХН3
Steel АЦ25ХГТ
AC30 steel
AC30X steel
АЦ30Х3МФ steel
АЦ30ХМ steel
AC35 steel
Steel АЦ18ХН2Т
AC35X steel
АЦ38ХС steel
AC40 steel
Steel AC40G
АЦ40Х steel
AC45 steel
Steel AC45G2
AC45X steel
AC50 steel
Steel AC50X
AC20CrNiM steel
A11 steel
A12 steel
A20 steel
A30 steel
A35 steel
A40G steel
AC12CrN steel
AC14 steel
AC14CrN steel
AC19CrN steel
AC20 steel
AC30CrM steel
AC35G2 steel
AC38CrHm steel
AC40 steel
AC40X steel
AC40CrNiM steel
AC45G2 steel
Steel ACS30CrM
АЦ18ХГТ steel
Designation
Name | The value |
---|---|
Designation GOST Cyrillic | АС40 |
Designation GOST Latin | AC40 |
Transliteration | AS40 |
The chemical elements | - |
Description
Steel AS40 used: for the manufacture of hammer stamps, bandages and matrices.
Note
Lead-carbon steel high machinability.
Standards
Name | Code | Standards |
---|---|---|
Sectional and shaped rolling | В32 | GOST 1414-75, GOST 14955-77 |
Chemical composition
Standard | C | S | P | Mn | Cr | Si | Ni | Fe | Cu | Pb |
---|---|---|---|---|---|---|---|---|---|---|
GOST 1414-75 | 0.37-0.45 | ≤0.04 | ≤0.04 | 0.5-0.8 | ≤0.25 | 0.17-0.37 | ≤0.25 | The rest | ≤0.25 | 0.15-0.3 |
Fe is the basis.
In accordance with GOST 1414-75, by agreement with the consumer, replacement of lead with selenium is allowed. In this case, the amount of selenium should be 2.5 times less than that of lead.
In accordance with GOST 1414-75, by agreement with the consumer, replacement of lead with selenium is allowed. In this case, the amount of selenium should be 2.5 times less than that of lead.
Mechanical characteristics
Section, mm | sT|s0,2, MPa | σB, MPa | d5, % | Brinell hardness number, MPa |
---|---|---|---|---|
Bars up to 100 mm. Normalization | ||||
25 | ≥335 | ≥570 | ≥19 | ≤187 |
Description mechanical marks
Name | Description |
---|---|
Section | Section |
sT|s0,2 | Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2% |
σB | Limit short-term strength |
d5 | Elongation after rupture |