Steel AS14

Designation

Name The value
Designation GOST Cyrillic АС14
Designation GOST Latin AC14
Transliteration AS14
The chemical elements -

Description

The AS14 steel is used: for the manufacture of propovednik and superheating pipe installations, high pressure with long life at temperatures up to +700 °C; shaped sections of high precision.

Note

The austenitic steel.
Serotonergically lead-containing steel of high machinability.

Standards

Name Code Standards
Sectional and shaped rolling В32 GOST 1414-75, GOST 14955-77, TU 14-1-1069-74, TU 14-1-512-90, TU 14-1-1256-91, TU 14-1-1271-75
Bulls. Blanks. Slabs В31 TU 14-1-1515-75, TU 14-1-904-74, TU 14-1-878-74
Tapes В34 TU 14-1-258-72

Chemical composition

Standard C S P Mn Cr Si Ni Fe Cu Pb
GOST 1414-75 0.1-0.17 0.15-0.3 ≤0.1 1-1.3 ≤0.25 ≤0.12 ≤0.25 The rest ≤0.25 0.15-0.3
TU 14-1-1271-75 0.1-0.17 ≤0.25 ≤0.1 1-1.3 - ≤0.1 - The rest - 0.15-0.3
Fe is the basis.

Mechanical characteristics

Section, mm sT|s0,2, MPa σB, MPa d5, % Brinell hardness number, MPa
The hot rolled, without heat treatment
- ≥410 ≥20 ≤170
Rental of calibrated and full hard without heat treatment
≥390 ≥490 ≥10 ≤207

Description mechanical marks

Name Description
Section Section
sT|s0,2 Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2%
σB Limit short-term strength
d5 Elongation after rupture