Alloy ХН58КТВЮМБЛ (ЧС104)
Alloy ZhS3LS
Alloy KhN63MYUTBV (SZHL-800; EK112)
Alloy KhN58KTVYUMBL (ChS104)
Alloy KhN58KVTYUMBL (ChS70; CH25)
Alloy KhN57KVYUTMBRL (ChS88U)
Alloy KhN57KVYUTMBL (ChS88)
Alloy KhN57VMTYUBL (ChS91)
Alloy KhN54MVTYUL (ChS94)
Alloy CrN35Zh14AMTL
Alloy LK4
Alloy L114
Alloy ZhS6K
Alloy ZhS3DK
Alloy VZHL2M
Alloy VZHL15
Alloy B56
Alloy B3K
Alloy Biduloid
Alloy 45X26H33S2B2
Alloy 45Х26Н23С2Б2
Alloy 12XH28MDTL (EI629)
Alloy 06Х20Н10М3Д3С4Л (06Х20Н10М3Д3С4)
Designation
Name | The value |
---|---|
Designation GOST Cyrillic | ХН58КТВЮМБЛ |
Designation GOST Latin | XH58KTBJuMBL |
Transliteration | HN58KTVYuMBL |
The chemical elements | CrNi58CoTeВAlCuBe |
Name | The value |
---|---|
Designation GOST Cyrillic | ЧС104 |
Designation GOST Latin | ChC104 |
Transliteration | ChS104 |
The chemical elements | ЧPb104 |
Description
Alloy ХН58КТВЮМБЛ used: for the production of cast bars in a vacuum-induction remelting for the manufacture of parts of power equipment and equipment for the shipbuilding industry, operating at temperatures up to +1000 °C.
Note
Alloy high-temperature and corrosion resistant Nickel-based.
Standards
Name | Code | Standards |
---|---|---|
Sectional and shaped rolling | В32 | TU 14-1-4787-90 |
Chemical composition
Standard | C | S | P | Mn | Cr | Si | Ni | Fe | Cu | N | As | Al | B | Ti | Mo | Sb | Pb | Bi | Nb | W | Zr | Co | Y | La |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
TU 14-1-4787-90 | 0.07-0.14 | ≤0.008 | ≤0.008 | ≤0.3 | 20-21.8 | ≤0.3 | The rest | ≤0.5 | ≤0.1 | ≤0.01 | ≤0.0005 | 2.1-2.9 | 0.015 | 3.1-3.9 | 0.3-0.9 | ≤0.0005 | ≤0.001 | ≤5.0E-5 | 0.15-0.35 | 3-4 | 0.03 | 10.3-12 | 0.03 | 0.02 |
Ni is the basis.
According to TU 14-1-4787-90 the chemical composition is given for the alloy of grade ХН58КТЮЮМБЛ-ВИ (ЧС104-ВИ). Boron, zirconium, yttrium and lanthanum are introduced by calculation, chemical analysis is not determined, but the calculated data are entered in the certificate. It is possible to estimate the mass fraction of arsenic in scores on the scale of spectral analysis. In this case, the mass fraction of arsenic should not be more than 1 point.
According to TU 14-1-4787-90 the chemical composition is given for the alloy of grade ХН58КТЮЮМБЛ-ВИ (ЧС104-ВИ). Boron, zirconium, yttrium and lanthanum are introduced by calculation, chemical analysis is not determined, but the calculated data are entered in the certificate. It is possible to estimate the mass fraction of arsenic in scores on the scale of spectral analysis. In this case, the mass fraction of arsenic should not be more than 1 point.