Description
Alloy AO12−1 is used: for bimetallic strip steel by rolling.
Note
The recommended modes of operation:
— load ≤ 29,5 Mn/m2 (300 kgf/cm2);
— sliding speed ≤ 20 m/s;
temperature ≤ 120 °C;
— recommended shaft hardness ≥ 250 HB.
On an antifriction layer of articles coated with a soft metal or a polymer antifriction coating thickness of from 0.003 to 0.03 mm. permitted by agreement with the consumer in technically justified cases to cover the product with a soft metal or polymer coating.
Standards
Name | Code | Standards |
---|---|---|
Non-ferrous metals, including rare metals, and their alloys | В51 | GOST 14113-78 |
Chemical composition
Standard | Ni | Fe | Cu | Al | Sn |
---|---|---|---|---|---|
GOST 14113-78 | 0.4-0.6 | ≤0.3 | 0.8-1.2 | The rest | 11-14 |
Al is the base.
According to GOST 14113-78, the content of other impurities, individually, should be ≤ 0.050%, and the total content of other impurities should be ≤ 0.55%.
According to GOST 14113-78, the content of other impurities, individually, should be ≤ 0.050%, and the total content of other impurities should be ≤ 0.55%.