By visiting this site, you accept the use of cookies. More about our cookie policy.

Steel N50

Designation

Name The value
Designation GOST Cyrillic Н50
Designation GOST Latin H50
Transliteration N50
The chemical elements Н50

Description

Steel N50 is used: for the manufacture of rails type R18 and R24 designed for installation on the Railways narrow gauge.

Note

Steel for the manufacture of rails is made with a degree of deoxidation SP (quiet) or SS (semi-killed).

Standards

Name Code Standards
Rails. Lining. Lining. Crutches В42 GOST 5876-82, GOST 6368-82

Chemical composition

Standard C S P Mn Si Fe As
GOST 5876-82 0.4-0.55 ≤0.045 ≤0.04 0.5-1.4 ≥0.13 The rest ≤0.15
Fe is the basis.
According to GOST 5876-82 in the steel smelted on the basis of Kerch ores, a mass fraction of sulfur and phosphorus is allowed up to 0.050%.

Mechanical characteristics

Section, mm σB, MPa Brinell hardness number, MPa
Mechanical properties of steel N50sp or N50ps for rails type R18 and R24 according to GOST 5876-82 on delivery
≥570 ≥170

Description mechanical marks

Name Description
Section Section
σB Limit short-term strength