By visiting this site, you accept the use of cookies. More about our cookie policy.

Steel 75

Designation

Name The value
Designation GOST Cyrillic 75
Designation GOST Latin 75
Transliteration 75
The chemical elements 75

Description

75 steel is used: for the manufacture of round and flat springs of various sizes, valve springs car engine, spring shock absorbers, springs, locking washers, clutch discs, Cams, spindles, shims and other parts operating in conditions of friction and under the action of static loads and vibration loads; knives earthmoving machinery (bulldozers, scrapers, graders and graders, as well as to the dozer and grader blades equipment excavators, rollers and other earth moving machines).

Note

Steel spring carbon.

Standards

Name Code Standards
Sectional and shaped rolling В22 GOST 1133-71, GOST 17152-89, GOST 2590-2006, GOST 2591-2006, GOST 2879-2006
Sheets and stripes В33 GOST 4405-75
Steel wire medium- and high-carbon В72 GOST 7348-81, GOST 9389-75, GOST 26366-84
Sectional and shaped rolling В32 GOST 7417-75, GOST 7419-90, GOST 8559-75, GOST 8560-78, GOST 14955-77, GOST 14959-79, TU 14-1-2118-77, TU 14-11-245-88, TU 14-1-1271-75, TU 14-136-367-2008
Sheets and stripes В23 GOST 82-70, GOST 103-2006

Chemical composition

Standard C S P Mn Cr Si Ni Fe Cu
GOST 17152-89 (ИСО 7129-82 0.72-0.8 ≤0.035 ≤0.035 0.5-0.8 ≤0.25 0.17-0.37 ≤0.25 The rest ≤0.2
GOST 14959-79 0.72-0.8 ≤0.035 ≤0.035 0.5-0.8 ≤0.25 0.17-0.37 ≤0.25 The rest ≤0.2
Fe is the basis.

Mechanical characteristics

Section, mm sT|s0,2, MPa σB, MPa d5, % y, %
Rolled steel. Steel categories: 3, 3A, 3B, 3C, 3D, 4, 4A, 4B. Quenching in oil from 820 °C to + Vacation at 470 °C
≥885 ≥1080 ≥9 ≥30

Description mechanical marks

Name Description
Section Section
sT|s0,2 Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2%
σB Limit short-term strength
d5 Elongation after rupture
y The relative narrowing

Physical characteristics

Temperature Е, ГПа G, ГПа
0 191 78

A description of the physical symbols

Name Description
Е The normal elasticity modulus
r Density
l Coefficient of thermal conductivity
R UD. the resistivity

Technological properties

Name The value
Weldability does not apply to welded structures. The CCC followed by heat treatment.
Propensity to temper brittleness tend not
Forging temperature Start - 1180 °C, the end - of 800 °C. the cross Section up to 220 mm are cooled in the wells.
Flock-sensitive sensitivity insensitive