Steel 15GF
Designation
| Name |
The value |
| Designation GOST Cyrillic |
15ГФ |
| Designation GOST Latin |
15GF |
| Transliteration |
15GF |
| The chemical elements |
15MnV |
Description
Steel 15GF used: for the production of sheet welded structures of car building.
Note
Low alloy steel manganese-vanadium. The degree of deoxidation — SP.
Steel 15GF provides strength class long products, strip and shaped rolled CP 325 with a thickness up to 32 mm., KP 345 at a thickness of from 10 to 20 mm., KP 375 in thicknesses up to 10 mm.
Steel 15GF provides strength grade sheet, universal broadband rental and roll-formed profiles KP 325 with plate thickness of from 20 to 32 mm., KP KP 345 and 355 with a thickness of 10 to 20 mm., KP 375 in thicknesses up to 10 mm. without the use of additional hardening treatment.
Standards
| Name |
Code |
Standards |
| Classification, nomenclature and general norms |
В20 |
GOST 19281-89 |
| Pipes steel and connecting parts to them |
В62 |
GOST 20295-85, GOST 24950-81 |
| Sheets and stripes |
В23 |
GOST 82-70, GOST 17066-94, GOST 19282-73 |
| Sectional and shaped rolling |
В22 |
GOST 8278-83, GOST 8281-80, GOST 8282-83, GOST 8283-93, GOST 9234-74, GOST 11474-76 |
| Sheets and stripes |
В33 |
TU 14-1-4431-88 |
| Sectional and shaped rolling |
В32 |
TU 14-136-367-2008 |
Chemical composition
| Standard |
C |
S |
P |
Mn |
Cr |
Si |
Ni |
Fe |
Cu |
N |
As |
Al |
V |
Ti |
Nb |
| GOST 17066-94 |
0.12-0.18 |
≤0.04 |
≤0.035 |
0.9-1.2 |
≤0.03 |
0.17-0.37 |
≤0.3 |
The rest |
≤0.3 |
≤0.008 |
≤0.08 |
≤0.03 |
0.05-0.1 |
≤0.03 |
≤0.03 |
| GOST 19282-73 |
0.12-0.18 |
≤0.04 |
≤0.035 |
0.9-1.2 |
≤0.03 |
0.17-0.37 |
≤0.3 |
The rest |
≤0.3 |
≤0.008 |
≤0.08 |
≤0.05 |
0.05-0.12 |
≤0.03 |
- |
Fe is the basis.
According to GOST 17066-94, the mass fraction of arsenic is allowed up to 0.015%, with the mass fraction of phosphorus being not more than 0.030%.
According to GOST 19282-73, it is allowed to modify steel with calcium and rare-earth elements from the calculation of the introduction of not more than 0.02% calcium and 0.05% rare-earth elements into the metal.
According to GOST 19281-89 and GOST 19282-73, it is allowed to add aluminum and titanium from the calculation of the mass fraction in the rolled aluminum - no more than 0.050%, titanium - no more than 0.030%.
Mechanical characteristics
| Section, mm |
sT|s0,2, MPa |
σB, MPa |
d5, % |
d4 |
| Steel hot-rolled sheet in the delivery condition |
| ≤10 |
≥380 |
≥520 |
≥21 |
- |
| 10-32 |
≥340 |
≥480 |
≥21 |
- |
| Bars and shapes of high-strength steel in the delivery state according to the GOST 19281-89 (specified strength class) |
| ≤32 |
≥325 |
≥450 |
≥21 |
- |
| 10-20 |
≥345 |
≥480 |
≥21 |
- |
| ≤10 |
≥375 |
≥510 |
≥21 |
- |
| The plates and universal broadband in the state of delivery GOST 19282-73 |
| ≤10 |
≥375 |
≥510 |
≥21 |
- |
| 10-20 |
≥355 |
≥510 |
≥21 |
- |
| Pre-painted steel sheet of high-strength steel in the delivery state GOST 17066-94 |
| 0.5-3.9 |
≥355 |
≥510 |
- |
≥18 |
| The plates and universal broadband in the state of delivery GOST 19282-73 |
| 20-32 |
≥335 |
≥470 |
≥21 |
- |
| Pre-painted steel sheet of high-strength steel in the delivery state GOST 17066-94 |
| 0.5-3.9 |
≥355 |
≥480 |
- |
≥18 |
Description mechanical marks
| Name |
Description |
| Section |
Section |
| sT|s0,2 |
Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2% |
| σB |
Limit short-term strength |
| d5 |
Elongation after rupture |
| d4 |
Elongation after rupture |
Technological properties
| Name |
The value |
| Weldability |
without restrictions |
| Propensity to temper brittleness |
tend not |
| Flock-sensitive sensitivity |
not sensitive |