Steel R9M4K8
Designation
Name |
The value |
Designation GOST Cyrillic |
Р9М4К8 |
Designation GOST Latin |
P9M4K8 |
Transliteration |
R9M4K8 |
The chemical elements |
- |
Description
R9M4K8 steel is used: for the manufacture of tools used in the processing of high-strength stainless and heat resisting steels, alloys and superior alloy steels in terms of increased heating of the cutting edge (cutting tool, milling cutters, shaped cutters, core drills, taps).
Note
Steel has a high tendency to decarburization.
Standards
Name |
Code |
Standards |
Sectional and shaped rolling |
В22 |
GOST 1133-71, GOST 2590-2006, GOST 2591-2006 |
Sheets and stripes |
В33 |
GOST 4405-75 |
Sectional and shaped rolling |
В32 |
GOST 7417-75, GOST 14955-77, GOST 19265-73, TU 14-11-245-88 |
Chemical composition
Standard |
C |
S |
P |
Mn |
Cr |
Si |
Ni |
Fe |
Cu |
V |
Mo |
W |
Co |
GOST 19265-73 |
1-1.1 |
≤0.03 |
≤0.03 |
0.2-0.5 |
3-3.6 |
0.2-0.5 |
≤0.6 |
The rest |
≤0.25 |
2.3-2.7 |
3.8-4.3 |
8.5-9.5 |
7.5-8.5 |
Fe is the basis.
Mechanical characteristics
Section, mm |
sT|s0,2, MPa |
σB, MPa |
d5, % |
y, % |
Rolled steel. Delivery condition |
|
≥540 |
≥960 |
≥7 |
≥10 |
Description mechanical marks
Name |
Description |
Section |
Section |
sT|s0,2 |
Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2% |
σB |
Limit short-term strength |
d5 |
Elongation after rupture |
y |
The relative narrowing |
Physical characteristics
Temperature |
Е, ГПа |
G, ГПа |
r, кг/м3 |
l, Вт/(м · °С) |
0 |
229 |
87 |
8300 |
- |
20 |
229 |
- |
8300 |
- |
100 |
- |
- |
- |
25 |
200 |
- |
- |
- |
27 |
300 |
- |
- |
- |
28 |
400 |
- |
- |
- |
29 |
500 |
- |
- |
- |
30 |
600 |
- |
- |
- |
31 |
700 |
- |
- |
- |
32 |
900 |
- |
- |
- |
32 |
A description of the physical symbols
Name |
Description |
Е |
The normal elasticity modulus |
r |
Density |
l |
Coefficient of thermal conductivity |
R |
UD. the resistivity |
Technological properties
Name |
The value |
Forging temperature |
Start - 1180 °C, the end - 880 °C. Cooling in the wells at 750-800 C. |
Grindability |
Reduced |
Viscosity |
reduced |
Resistance to wear |
increased |