By visiting this site, you accept the use of cookies. More about our cookie policy.

Steel R6M5K5

Designation

Name The value
Designation GOST Cyrillic Р6М5К5
Designation GOST Latin P6M5K5
Transliteration R6M5K5
The chemical elements -

Description

R6M5K5 steel is used: for the manufacture of roughing to semi-finishing tool used in the processing of superior alloy and stainless steels.

Note

Steel has a high tendency to decarburization.

Standards

Name Code Standards
Sectional and shaped rolling В22 GOST 1133-71, GOST 2590-2006, GOST 2591-2006
Sheets and stripes В33 GOST 4405-75
Sectional and shaped rolling В32 GOST 7417-75, GOST 14955-77, GOST 19265-73, TU 14-11-245-88
Steel wire medium- and high-carbon В72 TU 14-1-2783-79

Chemical composition

Standard C S P Mn Cr Si Ni Fe Cu V Mo W Co
GOST 19265-73 0.86-0.94 ≤0.03 ≤0.03 0.2-0.5 3.8-4.3 0.2-0.5 ≤0.6 The rest ≤0.25 1.7-2.1 4.8-5.3 5.7-6.7 4.7-5.2
Fe is the basis.

Mechanical characteristics

Section, mm sT|s0,2, MPa σB, MPa d5, % y, %
Rolled steel. Delivery condition
≥510 ≥850 ≥12 ≥14

Description mechanical marks

Name Description
Section Section
sT|s0,2 Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2%
σB Limit short-term strength
d5 Elongation after rupture
y The relative narrowing

Physical characteristics

Temperature Е, ГПа G, ГПа r, кг/м3 l, Вт/(м · °С) R, НОм · м
0 220 83 8200 - 458
20 220 - 8200 - 458
100 - - - 27 -
200 - - - 28 -
300 - - - 29 -
400 - - - 30 -
500 - - - 32 -
600 - - - 36 -
700 - - - 34 -
900 - - - 29 -

A description of the physical symbols

Name Description
Е The normal elasticity modulus
r Density
l Coefficient of thermal conductivity
R UD. the resistivity

Technological properties

Name The value
Forging temperature Start - 1160 °C, the end - 850 °C.
Grindability good
Viscosity good
Resistance to wear increased

Our consultant will save your time