By visiting this site, you accept the use of cookies. More about our cookie policy.

Alloy 33Н5Х

Designation

Name The value
Designation GOST Cyrillic 33Н5Х
Designation GOST Latin 33H5X
Transliteration 33N5H
The chemical elements 33Ni5Cr

Description

Alloy 33Н5Х used: for the production of strips and sheets cold-rolled, forged bars, used in the manufacture of magnetic shunts, parts, temperature relay and sensor heating.

Standards

Name Code Standards
Classification, nomenclature and general norms В30 TU 14-1-4478-88

Chemical composition

Standard C S Mn Cr Si Ni Fe Cu Al Ca Mg
TU 14-1-4478-88 ≤0.05 ≤0.02 0.2-0.4 4.3-5.1 ≤0.18 32.5-33.8 The rest ≤0.05 ≤0.05 ≤0.025 ≤0.05
Fe is the basis.

Technological properties

Name The value
Features of heat treatment Recommended heat treatment after the fabrication of parts or specimens for magnetic tests: annealing in vacuum not worse than 10-3 mm of mercury.St. at a temperature of 900 °C with exposure for 2 hours, cooled to 600-650 °C with a speed of 80-120 °C/hour, up to 300-350 °C, at a speed of 30-70 °C/hour, up to 100-150 °C with the switched off oven, then in air.