Cast Iron S-NiSiCr20-5-2
Designation
Name |
The value |
Designation GOST Cyrillic |
S-NiSiCr20-5-2 |
Designation GOST Latin |
S-NiSiCr20-5-2 |
Transliteration |
S-NiSiCr20-5-2 |
The chemical elements |
S-NiSiCr20-5-2 |
Description
Cast iron S-NiSiCr20−5-2 is used: for the manufacture of casting parts of valves, pumps, castings used in industrial furnaces that are subject to high mechanical stress.
Note
Nickel cast iron. Has good corrosion resistance even in diluted sulphuric acid, good heat resistance.
Standards
Name |
Code |
Standards |
Castings with special properties (cast iron and steel) |
В83 |
GOST 7769-82 |
Chemical composition
Standard |
C |
P |
Mn |
Cr |
Si |
Ni |
Fe |
Cu |
GOST 7769-82 |
≤3 |
≤0.08 |
0.5-1.5 |
1-2.5 |
4.5-5.5 |
18-22 |
The rest |
≤0.5 |
Fe is the basis.
Mechanical characteristics
sT|s0,2, MPa |
σB, MPa |
d4 |
Brinell hardness number, MPa |
Castings on OST 1 90077-72 |
210-260 |
370-430 |
10-18 |
180-230 |
Description mechanical marks
Name |
Description |
sT|s0,2 |
Yield strength or limit of proportionality with a tolerance for residual deformation of 0.2% |
σB |
Limit short-term strength |
d4 |
Elongation after rupture |
Physical characteristics
Temperature |
Е, ГПа |
20 |
112-133 |
A description of the physical symbols
Name |
Description |
r |
Density |
l |
Coefficient of thermal conductivity |
a |
The coefficient of linear expansion |