Alloy Ca4m1o (CAM4-1o)
Designation
Name |
The value |
Designation GOST Cyrillic |
ЦА4М1о |
Designation GOST Latin |
TsA4M1o |
Transliteration |
TsA4M1o |
The chemical elements |
ZnAl4Cu1о |
Name |
The value |
Designation GOST Cyrillic |
ЦАМ4-1о |
Designation GOST Latin |
TsAM4-1o |
Transliteration |
TsAM4-1o |
The chemical elements |
ZnAlCu4-1о |
Description
Alloy Ca4m1o applies: for injection molding of critical hull, reinforcing, decorative parts of automobile, tractor, electrical and other industries.
Note
Alloy high purity (the letter «o» at the end indicate the marks).
The alloy has good fluidity, good corrosion resistance, practically does not change size during natural aging.
Standards
Name |
Code |
Standards |
Non-ferrous metals, including rare metals, and their alloys |
В51 |
GOST 19424-97, GOST 25140-93 |
Chemical composition
Standard |
Si |
Fe |
Cu |
Al |
Zn |
Sn |
Pb |
Mg |
Cd |
GOST 19424-97 |
≤0.015 |
≤0.05 |
0.7-1.2 |
3.9-4.3 |
The rest |
≤0.001 |
≤0.004 |
0.03-0.06 |
≤0.002 |
GOST 25140-93 |
≤0.015 |
≤0.06 |
0.7-1.3 |
3.5-4.5 |
The rest |
≤0.001 |
≤0.005 |
0.02-0.06 |
≤0.003 |
Zn is the basis.
According to GOST 19424-97 in the alloy for the production of pigs, the mass fraction of the main components and specific impurities can be changed by agreement of the consumer with the manufacturer.
According to GOST 25140-93, the total mass fraction of lead, cadmium and tin should be ≤ 0.009%.
Mechanical characteristics
Section, mm |
σB, MPa |
d5, % |
Brinell hardness number, MPa |
Castings according to GOST 25140-93 |
|
≥215 |
≥1 |
≥80 |
|
≥270 |
≥1.7 |
≥80 |
Description mechanical marks
Name |
Description |
Section |
Section |
σB |
Limit short-term strength |
d5 |
Elongation after rupture |
Physical characteristics
Temperature |
r, кг/м3 |
l, Вт/(м · °С) |
a, 10-6 1/°С |
С, Дж/(кг · °С) |
20 |
6700 |
109 |
- |
440 |
100 |
- |
- |
265 |
- |
A description of the physical symbols
Name |
Description |
Е |
The normal elasticity modulus |
l |
Coefficient of thermal conductivity |
R |
UD. the resistivity |